Reducing Contact Resistance and Preventing Corrosion on Hard Chrome Plating Lines

November 16, 2026

Latest company case about Reducing Contact Resistance and Preventing Corrosion on Hard Chrome Plating Lines
A precision metal parts plater operates a hard chrome plating line with shared anodising stations. Cathode bars, anode bars, rack pick-up shoes and Cu/Al busbar joints are continuously exposed to chromic acid mist, alkaline cleaners and high humidity.
Previously, operators only abraded the contacts periodically without any interface protection. Over time, the following issues appeared:
  • Contact surfaces darkened, copper oxide formed, and contact resistance gradually increased.
  • The rectifier could not reach target current; tank voltage ran higher than expected.
  • Rack contacts showed intermittent connection, causing uneven coating thickness and edge burning.
  • Ordinary grease formed a skin, absorbed plating solution and created local insulation.
Solution
The plant reconditioned cathode bars, anode bars, pick-up shoes and busbar joints as follows:
  1. Clean contacts with Electrolube Ultrasolve (ULS) to remove oil and old compound.
  2. Lightly abrade with a non-woven pad until oxidation is loosened.
  3. Apply a thin film of Electrolube EPC electro-plating compound; its mild abrasive action helps displace tarnish and air gaps.
  4. Wipe off contaminated compound and immediately re-apply a clean thin layer before reassembly and torquing.
  5. Inspect every 1–2 months and repeat routine maintenance as needed.
EPC uses a complex ester base oil with clay thickener, NLGI 1 consistency, service range –40 to +135 °C. It is not absorbed by plating electrolytes and does not leave an insulating film like ordinary mineral grease.
Results
  • Contact resistance stayed more stable, tank voltage fluctuation reduced, and current response became more linear at a given rectifier voltage.
  • Discolouration and verdigris on copper bars reduced; cleaning frequency moved from weekly to monthly.
  • Intermittent rack contact decreased, improving hard chrome thickness uniformity.
  • No greasy skinning on busbar joints and no plating-solution absorption.
  • Only a thin film is required, so consumption is low and there is no run-off during use.
Suitable Locations
  • Cathode and anode bars
  • Rack pick-up shoes, rack contacts
  • Rectifier output busbar joints
  • Conductive rails in anodising lines